common problems and solutions of the dispensing control system process

Dec 03, 2020 Leave a message

1, the parting control system components offset;
  Phenomenon: Curing component shift, in severe cases, component pin is not on the pad.
  Cause: patch film out of the amount of uneven glue (e.g. chip element two pieces of glue one more one less), patch when the component shift, patch adhesive force decreased, after the tap PCB placement time is too long glue semi-curing.
  Solution: Check the adhesive nozzle for blockage, exclude the unevenness of the glue, adjust the working status of the patch machine, change the glue, dosage after the PCB placement time should not be too long (less than 4h).
  2, the dosing control system after curing the component pin floating / shifting;
  Phenomenon: After curing the component pins float up or shift, the tin material will enter the pad after peak welding, in severe cases of short circuit and open circuit.
  Causes: uneven patch film, too much patch film, patch when the component offset.
  Solution: Adjust the parameters of the dosing process, control the amount of dosing, adjust the parameters of the patch process.
  3, dosing control system to pull the wire / trailing tail;
  Phenomenon: Common defects in wire/tailing and dosing.
  Causes: the inner diameter of the adhesive mouth is too small, the tap pressure is too high, the pitch between the adhesive from the PCB is too large, the adhesive expired or the quality is not good, the film viscosity is too high, after removing from the refrigerator can not be restored to room temperature, the amount of glue is too much.
  Solution: change the inner diameter of the larger nozzle, reduce the dosing pressure, adjust the "stop" height, change the glue, choose suitable for viscosity of the glue, removed from the refrigerator should be restored to room temperature (about 4h), adjust the amount of dosing.
  4, the dosing control system glue mouth blockage;
  Phenomenon: the amount of glue mouth is less live no glue out.
  Cause: not completely cleaned in the pinhole, patch film mixed with impurities, there is a hole phenomenon, incompatible glue mix.
  Solution: change clean needles, change better quality patch film, patch film number should not be mistaken.
  5, the dosing control system is empty;
  Phenomenon: Only the dosing action, no amount of glue.
  Cause: mixed bubbles, glue mouth blockage.
  Solution: The glue in the syringe should be de-bubbled (especially its own glue), according to the glue mouth blocking method.
  6, the pointing control system curing, component bonding strength is not enough, peak welding will fall off;
  Phenomenon: after curing component bonding strength is not enough, lower than the specification value, sometimes by hand touch will appear chip.
  Causes: after curing process parameters are not in place, especially the temperature is not enough, the component size is too large, heat absorption is large, the light curing lamp aging, the glue is not enough, the component /pcb is contaminated.
  Solution: Adjust the curing curve, especially to increase the curing temperature, usually the peak curing temperature of the thermo-curing glue is very critical, reaching the peak temperature can easily cause chip drop. For photo-curing glue, it should be observed whether the photo-curing lamp is aging, whether the lamp is blackened, the amount of glue, the component/pcb is contaminated.
 The above is for the dosing control system process of common problems and solutions, only for your reference.